Frit A 1316

Reimbold & Strick lead monosilicate frit

OxideAnalysisFormula
PbO79.00%1.000
SiO221.00%0.987
Oxide Weight282.53
Formula Weight282.53
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 90 x 10-7 (20-400C)
GSPT - Frit Softening Point 470C
GTTM - Glass Transition Temperature 440C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 1316" descrip="Reimbold & Strick lead monosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="79.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="21.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved