Frit 37.960

Alternate Names: 37 960,37-960

OxideAnalysisFormula
MgO1.00%1.000
Al2O30.32%0.126
B2O31.09%0.631
SiO21.87%1.254
Oxide Weight172.48
Formula Weight172.48
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 1000-1120C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 37.960" descrip="" searchkey="37 960,37-960" loi="0.00" casnumber=""> <oxides> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.320" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="1.090" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="1.870" tolerance=""/> </oxides> </material>