Frit 37.528

Alternate Names: Frit 37 528, Frit 37-528

OxideAnalysisFormula
CaO7.32%0.500
MgO0.53%0.050
Na2O6.47%0.400
ZnO1.06%0.050
Al2O38.51%0.320
B2O314.34%0.789
SiO261.77%3.938
Oxide Weight383.13
Formula Weight383.13
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 940-1060C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 37.528" descrip="" searchkey="Frit 37 528, Frit 37-528" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.320" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.530" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.470" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.060" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.510" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.340" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.770" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved