Frit 37.062

Alternate Names: Frit 37 062, Frit 37-062

OxideAnalysisFormula
BaO29.60%0.461
CaO8.42%0.359
MgO0.58%0.034
K2O5.73%0.145
Al2O35.83%0.137
B2O34.23%0.145
SiO242.97%1.709
ZrO22.64%0.051
Oxide Weight239.01
Formula Weight239.01
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 980-1060C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 37.062" descrip="" searchkey="Frit 37 062, Frit 37-062" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="29.600" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.420" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.580" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.730" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.830" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.230" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="42.970" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="2.640" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved