Frit 35.690

Alternate Names: Frit 35 690, Frit 35-690

OxideAnalysisFormula
BaO12.12%0.260
CaO1.53%0.090
K2O2.00%0.070
Na2O0.57%0.030
ZnO1.24%0.050
PbO33.93%0.500
Al2O39.92%0.320
B2O31.06%0.050
SiO237.64%2.060
Oxide Weight328.97
Formula Weight328.97
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 1020-1140C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 35.690" descrip="" searchkey="Frit 35 690, Frit 35-690" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="12.120" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.530" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.570" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.240" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="33.930" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.920" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="1.060" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="37.640" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved