Frit 35.680

Alternate Names: Frit 35 680, Frit 35-680

OxideAnalysisFormula
CaO6.90%0.533
Na2O5.08%0.355
PbO5.72%0.111
Al2O38.10%0.344
B2O312.48%0.778
SiO261.73%4.455
Oxide Weight433.77
Formula Weight433.77
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 960-1080C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 35.680" descrip="" searchkey="Frit 35 680, Frit 35-680" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.900" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.080" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="5.720" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.480" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.730" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved