Frit 35.608

OxideAnalysisFormula
BaO0.92%0.573
PbO1.00%0.427
SiO20.63%1.000
Oxide Weight243.28
Formula Weight243.28
If this formula is not unified correctly please contact us.

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 35.608" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.920" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="0.630" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved