Frit 35.200

Alternate Names: 35 200, 35-200

OxideAnalysisFormula
BaO12.53%0.130
CaO3.97%0.113
MgO1.54%0.061
K2O0.51%0.009
Na2O2.70%0.070
ZnO23.50%0.461
PbO21.89%0.157
Al2O33.89%0.061
SiO229.47%0.783
Oxide Weight159.63
Formula Weight159.63
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 960-1040C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 35.200" descrip="" searchkey="35 200, 35-200" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="12.530" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.970" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.540" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.510" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.700" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="23.500" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="21.890" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.890" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="29.470" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved