Frit 35.108

Alternate Names: 35 108,35-108

OxideAnalysisFormula
CaO4.20%0.270
K2O1.31%0.050
Na2O2.41%0.140
PbO33.40%0.540
Al2O34.81%0.170
B2O34.24%0.220
SiO249.64%2.979
Oxide Weight360.68
Formula Weight360.68
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 920-1080C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 35.108" descrip="" searchkey="35 108,35-108" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.310" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.410" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="33.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.810" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.240" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.640" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved