Frit 35.075

Alternate Names: 35 075,35-075

OxideAnalysisFormula
CaO7.86%0.450
MgO1.51%0.120
K2O1.47%0.050
Na2O2.70%0.140
PbO16.68%0.240
Al2O38.89%0.280
B2O34.55%0.210
SiO256.34%3.010
Oxide Weight321.07
Formula Weight321.07
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 1020-1160C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 35.075" descrip="" searchkey="35 075,35-075" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.860" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.510" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.470" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.700" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="16.680" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.890" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.550" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.340" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved