Frit 34.030

Alternate Names: Frit 34 030, Frit 34-030

OxideAnalysisFormula
K2O1.22%0.040
Na2O0.40%0.020
PbO68.01%0.940
Al2O32.31%0.070
SiO228.05%1.440
Oxide Weight308.51
Formula Weight308.51
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 900-1080C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 34.030" descrip="" searchkey="Frit 34 030, Frit 34-030" loi="0.00" casnumber=""> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.220" tolerance="`"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.400" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="68.010" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.310" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="28.050" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved