Frit 33.170

OxideAnalysisFormula
CaO0.96%0.060
MgO0.92%0.080
K2O2.94%0.110
Na2O13.20%0.750
Al2O315.06%0.520
B2O37.51%0.380
SiO244.37%2.599
ZrO215.04%0.430
Oxide Weight352.05
Formula Weight352.05
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 1000-1100C

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 33.170" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.960" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.920" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.940" tolerance="`"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="15.060" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="7.510" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="44.370" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="15.040" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved