Frit 268-D

Zircon unleadled frit

Alternate Names: Frit FB-268-D

OxideAnalysisFormula
CaO1.00%0.057
K2O7.50%0.256
Na2O12.50%0.648
ZnO1.00%0.039
F2.50%0.423
Al2O37.50%0.236
B2O312.50%0.577
SiO242.50%2.271
ZrO27.50%0.195
Oxide Weight303.53
Formula Weight303.53
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 10.06

FRIT ID F2 SIO2 B2O3 Na2O K2O CaO Al2O3 ZrO2 ZnO CTE
FB268-D-2 1-5 40-45 10-15 10-15 5-10 0-2 5-10 10-15 0-2 10.06


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 268-D" descrip="Zircon unleadled frit" searchkey="Frit FB-268-D" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.000" tolerance="1"/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.500" tolerance="2.5"/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.000" tolerance="1"/> <oxide symbol="F" name="Fluorine" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.500" tolerance="2.5"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="42.500" tolerance="2.5"/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="7.500" tolerance="2.5"/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved