Frit 1817

High alkali leadless aluminun silicate frit

OxideAnalysisFormula
CaO13.96%0.406
MgO0.86%0.035
K2O4.79%0.083
Na2O18.10%0.476
P2O50.03%0.000
TiO20.04%0.001
Al2O38.46%0.135
SiO253.40%1.449
Fe2O30.37%0.004
Oxide Weight163.10
Formula Weight163.10
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1817" descrip="High alkali leadless aluminun silicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="13.960" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.860" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.790" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="18.100" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.030" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.040" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.460" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.400" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.370" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved