Frit 1451

Netherlands, Flanders area (Ferro?)

OxideAnalysisFormula
Na2O16.65%1.000
B2O337.20%1.990
SiO246.15%2.859
Oxide Weight372.37
Formula Weight372.37
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1451" descrip="Netherlands, Flanders area (Ferro?)" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="16.650" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="37.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.150" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved