Frit 1214

Barium manganese borosilicate low alumina frit

OxideAnalysisFormula
BaO14.10%0.333
CaO2.60%0.168
Li2O1.40%0.170
Na2O2.80%0.164
ZnO3.70%0.165
Al2O34.70%0.167
B2O319.10%0.995
SiO235.70%2.153
MnO215.90%0.663
Oxide Weight362.43
Formula Weight362.43
If this formula is not unified correctly please contact us.

Unknown European supplier


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1214" descrip="Barium manganese borosilicate low alumina frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="14.100" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.600" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="1.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.800" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="3.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="19.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="35.700" tolerance=""/> <oxide symbol="MnO2" name="Manganese Dioxide" status="" percent="15.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved