Frit 1213

Barium iron borosilicate low alumina frit

OxideAnalysisFormula
BaO18.80%0.505
CaO2.70%0.198
Li2O0.50%0.069
Na2O1.90%0.126
ZnO2.00%0.101
Al2O33.70%0.149
B2O317.00%1.006
SiO233.70%2.310
Fe2O319.60%0.505
Oxide Weight411.52
Formula Weight411.52
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1213" descrip="Barium iron borosilicate low alumina frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="18.800" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.700" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.900" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="33.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="19.600" tolerance=""/> </oxides> </material>