Frit 1210

Zinc alkali opacified alumina silicate frit

OxideAnalysisFormula
CaO4.00%0.279
Li2O0.50%0.066
K2O4.80%0.200
Na2O2.40%0.152
ZnO6.30%0.303
Al2O33.90%0.150
B2O319.70%1.109
SiO248.50%3.163
ZrO29.80%0.312
Oxide Weight391.55
Formula Weight391.55
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1210" descrip="Zinc alkali opacified alumina silicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.000" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.400" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="6.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.900" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="19.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.500" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="9.800" tolerance=""/> </oxides> </material>