Frit 1209

Calcium borate frit with very low alumina, silica

OxideAnalysisFormula
CaO40.70%1.000
Al2O32.20%0.030
B2O350.50%1.000
SiO26.50%0.149
Oxide Weight137.70
Formula Weight137.70
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1209" descrip="Calcium borate frit with very low alumina, silica" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="40.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.200" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="50.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="6.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved