Frit 1203

Alkali calcium very low boron alumina silicate frit

OxideAnalysisFormula
CaO8.70%0.299
K2O14.60%0.299
Na2O12.90%0.402
Al2O31.60%0.030
SiO262.20%1.997
Oxide Weight193.00
Formula Weight193.00
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1203" descrip="Alkali calcium very low boron alumina silicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.700" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="14.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved