Frit 1202

Alkali high calcium low boron low alumina frit

OxideAnalysisFormula
K2O19.60%0.499
Na2O5.20%0.201
ZnO10.20%0.300
Al2O36.40%0.150
B2O38.70%0.300
SiO250.00%1.994
Oxide Weight239.91
Formula Weight239.91
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1202" descrip="Alkali high calcium low boron low alumina frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="19.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.200" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved