Frit 1201

High zinc high potash high boron low silica frit

OxideAnalysisFormula
CaO14.60%0.389
Li2O2.50%0.125
K2O30.60%0.486
Al2O333.10%0.485
B2O310.30%0.221
SiO28.90%0.221
Oxide Weight149.48
Formula Weight149.48
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1201" descrip="High zinc high potash high boron low silica frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.600" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="2.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="30.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="33.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="10.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="8.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved