Frit 1047

High magnesia borosilicate frit

Alternate Names: 1047 Boraksfritte

OxideAnalysisFormula
CaO10.79%0.557
K2O2.41%0.074
Na2O7.91%0.369
Al2O317.85%0.507
B2O320.41%0.849
SiO240.63%1.957
Oxide Weight289.44
Formula Weight289.44
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit 1047" descrip="High magnesia borosilicate frit" searchkey="1047 Boraksfritte" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.790" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.410" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.910" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.850" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="20.410" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.630" tolerance=""/> </oxides> </material>