Fremington Clay

Oxide Analysis Formula
CaO 4.87% 0.37
K2O 3.98% 0.18
MgO 3.97% 0.42
Na2O 0.44% 0.03
TiO2 0.94% 0.05
Al2O3 20.11% 0.84
SiO2 59.68% 4.23
Fe2O3 6.01% 0.16
Oxide Weight 425.99
Formula Weight 425.99

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


CAPTCHA

Leave the following empty



https://digitalfire.com, All Rights Reserved
Privacy Policy