Forshammer Feldspar

Swedish feldspar

OxideAnalysisFormula
K2O4.20%0.365
Na2O4.80%0.635
Al2O314.50%1.165
SiO275.60%10.310
Fe2O30.14%0.007
LOI0.60
Oxide Weight813.41
Formula Weight818.32
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Forshammer Feldspar" descrip="Swedish feldspar" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.800" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="14.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="75.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.140" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.600" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved