FinnTalc

Hydrous Magnesium Calcium Silicate

OxideAnalysisFormula
MgO31.00%1.000
Al2O30.20%0.003
SiO261.00%1.319
FeO1.90%0.030
LOI5.40
Oxide Weight122.33
Formula Weight129.31
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="FinnTalc" descrip="Hydrous Magnesium Calcium Silicate" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="31.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.000" tolerance=""/> <oxide symbol="FeO" name="Ferrous Oxide" status="" percent="1.900" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="5.400" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved