Ferro Richoux Frit 21 C007

Alkaline Borate Frit

OxideAnalysisFormula
CaO6.27%0.287
K2O2.30%0.063
Na2O15.71%0.650
Al2O33.70%0.093
B2O32.58%0.095
SiO269.44%2.966
Oxide Weight256.69
Formula Weight256.69
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 900-1000C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Richoux Frit 21 C007" descrip="Alkaline Borate Frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.270" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.710" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.580" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.440" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved