Ferro Richoux Frit 21 C006

Alkaline Borate Frit

OxideAnalysisFormula
CaO4.77%0.210
K2O0.99%0.026
Na2O19.17%0.764
Al2O311.51%0.279
B2O310.74%0.381
SiO252.82%2.171
Oxide Weight247.08
Formula Weight247.08
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 850-1000C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Richoux Frit 21 C006" descrip="Alkaline Borate Frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.770" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.990" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="19.170" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.510" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="10.740" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.820" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved