Ferro Richoux Frit 21 C005

Fritte Alcaline

OxideAnalysisFormula
BaO8.29%0.105
CaO3.03%0.105
K2O10.18%0.210
Na2O18.51%0.580
Al2O34.88%0.093
B2O33.76%0.105
SiO251.35%1.660
Oxide Weight194.29
Formula Weight194.29
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 880-1060C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Richoux Frit 21 C005" descrip="Fritte Alcaline" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="8.290" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.030" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="10.180" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="18.510" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.880" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="3.760" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.350" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved