Ferro Richoux Frit 21 C004

Alkaline Borate Frit

Alternate Names: Frit 21 C004

OxideAnalysisFormula
CaO1.58%0.094
MgO0.22%0.018
K2O4.38%0.155
Na2O13.64%0.733
Al2O310.68%0.349
B2O317.06%0.817
SiO252.14%2.891
ZrO20.30%0.008
Oxide Weight333.20
Formula Weight333.20
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 900-1100C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Richoux Frit 21 C004" descrip="Alkaline Borate Frit" searchkey="Frit 21 C004" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.580" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.220" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.380" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.640" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.680" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.060" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.140" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved