Ferro Richoux Frit 21 C003

Fritte Boracique

Alternate Names: Frit 21 C003

OxideAnalysisFormula
CaO3.69%0.300
MgO2.21%0.250
Na2O5.43%0.400
ZnO0.89%0.050
Al2O36.70%0.300
B2O315.25%1.000
SiO265.83%4.999
Oxide Weight456.35
Formula Weight456.35
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 1030-1180C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Richoux Frit 21 C003" descrip="Fritte Boracique" searchkey="Frit 21 C003" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.690" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.210" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.430" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.890" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.250" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="65.830" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved