Ferro Richoux Frit 21 C002

Fritte Boracique

Alternate Names: Frit 21 C002

OxideAnalysisFormula
CaO8.57%0.351
MgO0.03%0.002
K2O8.72%0.213
Na2O11.74%0.435
Al2O39.01%0.203
B2O313.39%0.442
SiO248.53%1.854
Oxide Weight229.63
Formula Weight229.63
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 920-1050C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Richoux Frit 21 C002" descrip="Fritte Boracique" searchkey="Frit 21 C002" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.570" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.030" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="8.720" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="11.740" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.010" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.390" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.530" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved