•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

Ferro Richoux Frit 21 C001

Fritte Boracique

Alternate Names: Frit 21 C001

OxideAnalysisFormula
CaO27.09%1.000
Al2O34.78%0.097
B2O350.45%1.501
SiO217.68%0.609
Oxide Weight207.09
Formula Weight207.09
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.1 x 10-8 C
MLRG - Frit Melting Range (C) 1050-1160C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Richoux Frit 21 C001" descrip="Fritte Boracique" searchkey="Frit 21 C001" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="27.090" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.780" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="50.450" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="17.680" tolerance=""/> </oxides> </material>