Ferro Frit KGF4131

A medium to hard unleaded frit

Alternate Names: Frit KGF4131

Oxide Weight331.20
Formula Weight331.20
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 61 x 10-7 20-500C
GSPT - Frit Softening Point 670C
GTTM - Glass Transition Temperature 608C

The data sheet of a frit having a proprietary chemistry

The data sheet of a frit having a proprietary chemistry

Some frit companies publish the chemistry of their frits, others do not. Some publish some of their products. Some published in the past but do not do so now. When frit data sheets do not provide an oxide analysis they become an impediment to use in glaze chemistry.

Out Bound Links

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit KGF4131" descrip="A medium to hard unleaded frit" searchkey="Frit KGF4131" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.500" tolerance=""/> </oxides> </material>