•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

Ferro Frit FB-284-M

Barium Frit

Alternate Names: Frit 284M, FB284M, FB284-M, FB-284M

OxideAnalysisFormula
BaO27.40%0.668
Na2O5.50%0.332
Al2O35.40%0.198
B2O312.40%0.666
SiO247.50%2.955
ZrO21.80%0.055
Oxide Weight373.91
Formula Weight373.91
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 1500F

In 2014, this is the only barium frit that Ferro is selling.
Useful in barium matte floor tile glazes, partially fritted satin matte glazes.
Barium source for bright colors cone 05-03.
This is a replacement for Frit 3289, it has 1.8% ZrO2 in place of that much silica.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit FB-284-M" descrip="Barium Frit" searchkey="Frit 284M, FB284M, FB284-M, FB-284M" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="27.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.500" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="1.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved