Ferro Frit FB-276-P

Artware Glaze Frit

OxideAnalysisFormula
CaO7.50%0.506
MgO0.50%0.047
K2O0.50%0.020
Na2O2.50%0.153
SrO7.50%0.274
Al2O37.50%0.278
B2O312.50%0.680
SiO252.50%3.307
ZrO20.50%0.015
Oxide Weight346.43
Formula Weight346.43
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.09
GSPT - Frit Softening Point 1750F

Well balanced clear for colored cone 06-04 hobby glazes.

Ferro provides only approximate formula information:
It contains no lead, zinc, or barium.
Potash/soda/lithium: 5%
Calcium 8%
Strontium Carbonate 5-9%
Alumina 10%
Boron 10-15%
Silica 50-60%


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit FB-276-P" descrip="Artware Glaze Frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance="0.5"/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.500" tolerance=".5"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.500" tolerance="2.5"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.500" tolerance="2.5"/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.500" tolerance="0.5"/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved