Ferro Frit FB-276-P-2 (approx)

Strontium lithium borate frit

OxideAnalysisFormula
CaO7.50%0.397
Li2O2.50%0.249
MgO0.50%0.037
K2O2.50%0.079
Na2O0.50%0.024
SrO7.50%0.215
Al2O37.50%0.218
B2O312.50%0.533
SiO252.50%2.592
ZrO20.50%0.012
Oxide Weight278.94
Formula Weight278.94
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.09
MLRG - Frit Melting Range (C) 1750F

This is a Ferro USA pottery frit.

As of 2008, ferro provides only an approximate analysis (shown here).


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit FB-276-P-2 (approx)" descrip="Strontium lithium borate frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=".5"/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.500" tolerance=".5"/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.500" tolerance="2.5"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.500" tolerance="2.5"/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.500" tolerance=".5"/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved