Ferro Frit DA4193

Clear, hard barium borosilicate frit

OxideAnalysisFormula
BaO4.97%0.100
CaO9.27%0.510
K2O3.05%0.100
Na2O3.82%0.190
ZnO2.64%0.100
Al2O36.61%0.200
B2O313.98%0.620
SiO255.68%2.859
Oxide Weight308.62
Formula Weight308.62
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 590C
MLRG - Frit Melting Range (C) 1040-1100C
GTTM - Glass Transition Temperature 653C

Chemistry from frits page at Walker Ceramics


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit DA4193" descrip="Clear, hard barium borosilicate frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="4.970" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.270" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.050" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.820" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.640" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.610" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.980" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.680" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved