Ferro Frit CM-943

OxideAnalysisFormula
K2O0.30%0.010
Na2O2.70%0.130
ZnO7.60%0.279
PbO43.50%0.582
Al2O35.00%0.146
B2O35.00%0.214
SiO235.90%1.783
Oxide Weight298.51
Formula Weight298.51
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 1750F

Yellow leadless cadmium, underglaze mix; complete by itself. Works well with CM-942 to produce oranges. Cone 06.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit CM-943" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.700" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="7.600" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="43.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="35.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved