Ferro Frit CE VTR 29

Lead bisilicate frit

Alternate Names: Frit VTR 29, Frit VTR29

OxideAnalysisFormula
PbO65.00%1.000
SiO235.00%2.000
Oxide Weight343.38
Formula Weight343.38
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 980-1020C

Their web page does not give the chemistry, but does indicate the presence of Al2O3 and KNaO. We assume these are in small amounts since they call this a lead bisilicate.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit CE VTR 29" descrip="Lead bisilicate frit" searchkey="Frit VTR 29, Frit VTR29" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="65.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="35.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved