Ferro Frit CC-279-3 (approx)

Fluorine lithium strontium zircon borate frit

Alternate Names: Frit CC-279

OxideAnalysisFormula
CaO7.50%0.308
Li2O2.50%0.193
MgO0.50%0.029
K2O5.00%0.122
Na2O7.50%0.279
ZnO0.50%0.014
SrO2.50%0.056
F2.50%0.303
Al2O37.50%0.169
B2O317.50%0.579
SiO252.50%2.011
ZrO22.50%0.047
Oxide Weight249.82
Formula Weight249.82
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.32 x 10-6

This is a USA pottery frit.

Ferro only publishes an approximate analysis, that is shown here.
This is for fritted or highly fritted clear glazes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit CC-279-3 (approx)" descrip="Fluorine lithium strontium zircon borate frit" searchkey="Frit CC-279" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=".5"/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.000" tolerance="2.5"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.500" tolerance=".5"/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="F" name="Fluorine" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.500" tolerance="2.5"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.500" tolerance="2.5"/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="2.500" tolerance="2.5"/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved