Ferro Frit CC-266

Low COE. Early softening, late flow. Can stand alone or use to reduce crazing.

flow 1900
potassium oxide - <10
sodium oxide - <10
lithium dioxide - <10
aluminium oxide - 2-10
boron oxide - 15-30
silica - >50
C.E.O. - 5