Ferro Frit CC-263-2

GLAZE FRIT CONE 04-2

OxideAnalysisFormula
CaO7.50%0.653
MgO0.50%0.061
K2O2.50%0.130
Na2O0.50%0.039
SrO2.50%0.118
Al2O312.50%0.598
B2O317.50%1.228
SiO252.50%4.265
ZrO20.50%0.020
Oxide Weight471.12
Formula Weight471.12
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.79 x 10-6
GSPT - Frit Softening Point 1850F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit CC-263-2" descrip="GLAZE FRIT CONE 04-2" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=".5"/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.500" tolerance=".5"/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="2.500" tolerance="2.5"/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.500" tolerance="2.5"/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.500" tolerance="2.5"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.500" tolerance="2.5"/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.500" tolerance=".5"/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved