Ferro Frit CC-261

Zinc frit

Alternate Names: Frit CC261

OxideAnalysisFormula
ZnO10.90%1.000
Oxide Weight81.40
Formula Weight81.40
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.7

SiO2:Al2O3 ratio is 11.51
Alkalies: 5-15%
CaO 5-15%
MgO less than 5%
Al2O3 5-15%
B2O3 less than 5%
SiO2 over 50%


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit CC-261" descrip="Zinc frit" searchkey="Frit CC261" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved