Ferro Frit CC-251

Floor tile glazes

Alternate Names: Frit CC251

COLE - Co-efficient of Linear Expansion 4.57
GSPT - Frit Softening Point 1800F

One source specified SiO2:Al2O3 ratio of: 5.13