Ferro Frit CC-250-2

Calcium boron source for partially fritted glazes

OxideAnalysisFormula
CaO12.50%0.638
K2O0.50%0.015
Na2O7.50%0.347
Al2O312.50%0.351
B2O317.50%0.720
SiO252.50%2.502
Oxide Weight295.05
Formula Weight295.05
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.73 X 10-6
GSPT - Frit Softening Point 1500F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit CC-250-2" descrip="Calcium boron source for partially fritted glazes" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.500" tolerance="2.5"/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.500" tolerance=".5"/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.500" tolerance="2.5"/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.500" tolerance="2.5"/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.500" tolerance="2.5"/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.500" tolerance="2.5"/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved