Ferro Frit 5301

Very high expansion leadless fluorine frit

Alternate Names: F5301, Frit 501E34, Frit 5301-2

OxideAnalysisFormula
CaO2.36%0.129
K2O5.53%0.179
Na2O14.03%0.692
F9.00%1.448
Al2O312.08%0.362
B2O312.48%0.548
SiO244.49%2.263
Oxide Weight305.66
Formula Weight305.66
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 11.41 (50-450C)
MLRG - Frit Melting Range (C) 1400-1500F

This is a USA pottery frit, Ferro now calls it Frit 5301-2.
Formerly Frit 4101
The fluorine content seems to be impossibly high, likely an error.

Useful in high expansion crackle glazes at 06 or to deal with shivering in other glazes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 5301" descrip="Very high expansion leadless fluorine frit" searchkey="F5301, Frit 501E34, Frit 5301-2" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.360" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.530" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="14.030" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="9.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.080" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.480" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="44.490" tolerance=""/> </oxides> </material>