Ferro Frit 4712

Borosilicate hard clear general purpose frit 1040-1100C

Alternate Names: Frit 4712

OxideAnalysisFormula
CaO9.54%0.600
K2O3.47%0.130
Na2O4.74%0.270
Al2O310.12%0.350
B2O312.43%0.630
SiO259.66%3.500
Oxide Weight352.54
Formula Weight352.54
If this formula is not unified correctly please contact us.

General purpose and versatile frit, good for strong and underglaze colors.
New name is Frit 4113.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4712" descrip="Borosilicate hard clear general purpose frit 1040-1100C" searchkey="Frit 4712" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.548" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.474" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.748" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.126" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.438" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="59.666" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved