Ferro Frit 4616

High zinc borosilicate frit for matte glazes 1040-1100C

OxideAnalysisFormula
CaO4.60%0.150
K2O1.54%0.030
Na2O3.38%0.100
ZnO32.03%0.720
Al2O34.46%0.080
B2O310.27%0.270
SiO243.69%1.330
Oxide Weight182.94
Formula Weight182.94
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4616" descrip="High zinc borosilicate frit for matte glazes 1040-1100C" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.545" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.389" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="32.038" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.461" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="10.273" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.695" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved