Ferro Frit 4193

Transparent hard barium zinc borosilicate leadless frit

OxideAnalysisFormula
BaO2.04%0.043
CaO9.42%0.541
K2O2.94%0.100
Na2O3.97%0.206
ZnO2.78%0.110
Al2O36.87%0.217
B2O314.25%0.659
SiO257.73%3.092
Oxide Weight321.94
Formula Weight321.94
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 1040-1100C

Supposedly this used to be Frit 938 however, while very similar this only has half the amount of BaO.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Ferro Frit 4193" descrip="Transparent hard barium zinc borosilicate leadless frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.040" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.420" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.940" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.970" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.780" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.870" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.250" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.730" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved